DLP Modeling V3 Resins for SprintRay Printers
“
Specifications:
- Product Name: DLP SG Clear (DSP-SG001CR)
- Compatible with SprintRay printers: Pro 2, Pro S 95 & 55,
Pro95 & 55 - Layer Thickness: 50/100 Micron
- Material Options: SprintRay Try-In 2, SprintRay US, SprintRay
Surgical Guide 2, SprintRay Surgical Guide 3
Product Usage Instructions:
Pre-Printing Preparation:
- Ensure SG Resin is well shaken.
- Clean optical pathways and check resin tank condition.
Printing Process:
- Use RayWare Cloud or Desktop version 2.9.2 and later for
printing settings. - Select the appropriate job type, model type, printer, material,
and layer thickness. - After printing, remove parts and clean them in A&B IPA bath
(95% IPA). - Dry the models thoroughly with compressed air for a minimum of
25 minutes in a shaded location.
Post-Printing Steps:
- Ensure printed parts are completely free of IPA before UV
post-curing. - Avoid extended wash times or residual IPA to prevent
deformation and lower mechanical properties. - For sterilization, autoclave the models without the need for
longer or hotter cycles.
FAQ:
Q: How should I store Specialty Series printed models?
A: Store the models avoiding forces during cooling and maintain
them in a sterilized environment.
“`
APPLYLABWORK PRINTING TIPS
(Not endorsed by SprintRay)
DLP SG Clear
(DSP-SG001CR)
SprintRay printers
(Pro 2, Pro S 95 & 55, Pro95 & 55)
Checks: SG Resin is well shakened, Optical
pathways are clean, Resin tank condition.
RayWare Cloud:
Job Type: Dental Model Dental Model Type: Other Printer: Pro 2, Pro S 95, & Pro S 55 Material: SprintRay Try-In 2 Layer Thickness: 50/100 Micron
Cleaning: A&B IPA bath [fresh 95% IPA]
A-bath: Submerge freshed removed parts in A-bath. Swish the parts around in the IPA, with a gental dental brush to remove uncured resin on the surfaces. Transfer to B-bath. B-bath: Submerged for 3 mins.
Total IPA clean time should not exceed 5 minutes.
Blow dry the models with compressed air, let models sit dry completely, 25 mins minimum, in a shaded airy location. Printed parts must be free of IPA before UV post-curing. Extended wash time and residual IPA (if not dried completely) causes deformation and lower mechanical properties.
Post-Curing: · Pro Cure 1 (version 1.73 and later)
· Offset is an optional function that depends on the printer’s intensity variation.
· The recommended offset value is 0 µm.
RayWare Desktop: version 2.9.2 and later Pro S (95 & 55)
Material: SprintRay US Try-In 2 Layer Thickness 50/100 µm
Select Custom, then select the conditions as 30oC for 15 mins.
· Por Cure 2 (version 1.2.12 and later)
Pro (95 & 55)
Material: SprintRay US SprintRay Surgical Guide 2
Layer Thickness50/100/170 µm
Select Material Sprintray Surgical guide 3, and then select exposure zone.
· Nano Cure (Software version 1.0.9 and later)
For detailed calibration, please refer to Tips for dimension and tolerance testing
Avoid placing supports near the guide sleeve holes and on the intaglio surfaces. Inspect support locations to add or remove supports as needed.
Select Material SprintRay SprintRay Surgical guide 3, and then select Start.
Specialty Series
APPLYLABWORK PRINTING TIPS
(Not endorsed by SprintRay) Sterilization:
a. Models must be fully post-cured before autoclave. b. Autoclave: 15 mins at 121°C / 250°F. No stacking of
models in autosclave. Longer or hotter autoclave cycle is not needed. Color Change:
c. Allow the print to cool to room temperature. Avoid forces to the models during cooling.
Storage:
Keep the resin in the original bottle, room temperature (15-26°C / 59-79°F) in a dry and dark area. Filter out all debris in the case of fail print jobs.