ANDELI MIG-205DP

Contents

ANDELI MIG-205DP Multi-Process Welder

Instruction Manual

1. Introduction

Thank you for choosing the ANDELI MIG-205DP Multi-Process Welder. This machine is designed for versatility and high performance, offering 8-in-1 functionality including Pulsed MIG, Gas MIG, SYN/MAN MIG, HF TIG, CUT, Clean, Cold Welding, Spot Welding, and MMA Aluminum Welding. It is suitable for a wide range of applications from thin-sheet work to heavy-duty repairs.

For detailed information and safety guidelines, please refer to the complete user manual available as a PDF: ANDELI MIG-205DP User Manual (PDF).

2. Safety Information

WARNING: Read this manual thoroughly before installation, operation, or repair. Failure to do so may result in serious personal injury or loss of life.

2.1. General Safety Precautions

  • Electric Shock Can Kill: Do not touch electrically live parts. Wear dry, hole-free gloves and insulate yourself from the work and ground.
  • Fumes and Gases Can Be Dangerous: Avoid breathing fumes and gases. Use adequate ventilation or exhaust at the arc. Keep your head out of the fume plume.
  • Arc Rays Can Burn: Wear a welding helmet with the proper filter plate and protective clothing to protect eyes and skin from arc rays and spatter.
  • Welding and Cutting Sparks Can Cause Fire or Explosion: Remove fire hazards from the welding area. Have a fire extinguisher readily available. Do not weld or cut on containers that have held hazardous substances.
  • Cylinder May Explode If Damaged: Use only compressed gas cylinders with correct shielding gas and properly operating regulators. Secure cylinders in an upright position.
  • For Electrically Powered Equipment: Turn off power before working on equipment. Install equipment according to national and local electrical codes.

2.2. California Proposition 65 Warnings

WARNING: Breathing diesel engine exhaust exposes you to chemicals known to the State of California to cause cancer and birth defects, or other reproductive harm. Always start and operate the engine in a well-ventilated area.

WARNING: This product, when used for welding or cutting, produces fumes or gases which contain chemicals known to the State of California to cause birth defects and, in some cases, cancer. (California Health & Safety Code § 25249.5 et seq.)

WARNING: Cancer and Reproductive Harm www.P65warnings.ca.gov

2.3. Electric and Magnetic Fields (EMF)

Electric current flowing through any conductor causes localized Electric and Magnetic Fields (EMF). Welding current creates EMF fields around welding cables and welding machines. EMF fields may interfere with some pacemakers. Welders with pacemakers should consult their physician before welding. To minimize exposure, route electrode and work cables together, never coil the electrode lead around your body, and connect the work cable to the workpiece as close as possible.

3. Product Overview

The ANDELI MIG-205DP is an 8-in-1 multi-process IGBT inverter welder and cutter. It supports MIG (Pulse, Gas, Gasless, SYN, MAN), MMA (Stick), TIG (HF, Cold), CUT (Plasma), and Clean modes. This machine is designed for high efficiency and adaptability, suitable for various metal fabrication tasks.

ANDELI MIG-205DP Multi-Process Welder with all included accessories

Figure 3.1: ANDELI MIG-205DP Multi-Process Welder and included accessories.

3.1. Key Features

  • Multi-Process Capability: MIG (Pulse, Gas, Gasless, SYN, MAN), MMA, HF TIG, Cold TIG, Plasma CUT, and Weld Clean.
  • Smart Interface: Large 5-inch HD LED display for real-time data and intuitive rotary knob for parameter selection.
  • Advanced Control: MCU-based digital control for consistent, stable performance. Supports professional adjustments like inductance, slow wire feeding, pre/post gas timing, Initial/Finish Current, anti-stick, thrust, and VRD.
  • Aluminum Welding: Supports GMAW-S and Pulse MIG for aluminum alloys and carbon steel.
  • Dual Voltage: Operates on both 110V and 220V, 50/60 Hz power supplies.
  • High-Frequency Arc Start: Built-in HF arc start for TIG (non-contact) and HF pilot arc for plasma cutting (handles painted, rusty, uneven surfaces).
  • Cold Welding Mode: Exclusive TIG mode for low-heat welding, minimizing distortion on thin stainless/carbon steel.
  • Weld Cleaning Function: Dedicated function for post-weld seam cleaning, removing oxidation and discoloration.
  • Robust Protection: Optimized auto-protection against voltage fluctuation, overheating, and other abnormalities.
  • Portable Design: Weighs 12.8 kg with dimensions of 490*225*340MM, making it easy to carry.
5-inch larger LED display showing real-time welding data

Figure 3.2: 5-inch Larger LED Display for real-time data and crystal-clear visibility.

Diagram of the Advanced MCU Chip

Figure 3.3: Advanced MCU Chip for smart digital control and optimized auto protection.

4. Specifications

4.1. General Specifications

Attribute Value
Model Number MIG-205DP
Brand Name ANDELI
Power Supply Voltage 230V ±10% (Dual Voltage 110V/220V)
Frequency 50/60Hz
Dimensions (L*W*H) 490*225*340MM
Net Weight 12.8KG
Certification CE
IP Rating IP21S
Insulation Class H
Cooling Way FAN & AIR

4.2. Performance Specifications

Function Rated Input Capacity (KVA) Output Current Range (A) Duty Cycle (40°C 10min) Efficiency (%)
MIG 8.1 50-205 30%@205A, 60%@118A, 100%@92A 78
TIG 6.4 10-205 25%@205A, 60%@118A, 100%@92A 74
MMA 7.9 10-205 25%@205A, 60%@132A, 100%@103A 80
CUT 7.6 20-50 30%@40A, 60%@35A, 100%@27A 85

Note: The welding duty cycle is the percentage of actual continuous welding time that can occur in a ten minute cycle. For example: 25% at 200amps means the welder can weld continuously at 200 amps for 2.5 minutes and then the unit will need to be rested for 7.5 minutes.

Welding Quick Reference Chart for various parameters and material thickness

Figure 4.1: Welding Quick Reference Chart for MIG-205DP.

5. Setup

5.1. Wire Feeder Tension Adjustment

Proper wire feeder tension is crucial for smooth wire feeding. Too loose, and the spool may spin freely; too tight, and the drive roller may struggle to pull the wire, leading to slipping or premature wear.

  1. Open the welder door and remove the Spool Retaining Knob from the wire spool spindle.
  2. Slide the wire spool onto the center of the spindle, ensuring the drive pin engages with a spoke of the wire spool.
  3. Reinstall the Spool Retaining Knob.
  4. Gradually tighten the Spool Retaining Knob until there is slight resistance when spinning the wire spool on the spindle.

WARNING: Before changing the feed roller or wire spool, ensure that the mains power is switched off.

WARNING: Excessive feed tension can cause rapid and premature wear of the drive roller, support bearing, and drive motor.

5.2. MIG/MAG Welding Setup (GMAW)

The polarity adapter is located inside the machine. Wire as shown in MIG/MAG GAS mode.

  1. MIG Gun Connection: Connect the MIG gun to the Euro Torch Connector.
  2. Polarity Setup: Attach the Wire Drive Polarity Lead to the Positive (+) Output Terminal. Connect the work clamp to the Negative (-) Output Terminal, ensuring it's securely attached to clean, bare metal.
  3. Load Welding Wire: Install the wire spool into the cabinet. Feed the wire through the feeder and into the MIG torch.
  4. Gas System Connection: Attach the gas regulator to the gas cylinder. Connect the gas line to the regulator.
  5. Prime the Wire: Hold the torch trigger or the "Wire Check" button on the panel to feed the wire.
  6. Gas Flow Setup: Open the gas cylinder valve. Pull the trigger to verify gas flow and adjust the regulator to 20-30 CFH (cubic feet per hour).
  7. Power On & Process Selection: Turn on the machine. Select MIG/MAG Welding Process from the Home Menu. Navigate to the MIG/MAG Parameter Settings page.
  8. Parameter Setup: Select Wire Type (Steel, Stainless Steel, AL4043, AL5356), Gas Type (100% CO2, Mixed Gas, 100% Argon), and Wire Diameter (0.6mm-1.2mm). Set Trigger Mode to 2T, 4T, or Spot Welding.
  9. Final Checks: Confirm Standard MIG Torch Mode is active. Test wire feed by triggering the torch control switch. Start to weld.
Spool support for 2lb or 10lb MIG wire and pre-installed air filter regulator

Figure 5.1: Spool support for 2lb or 10lb MIG wire and pre-installed air filter regulator.

5.3. Aluminum Welding Torch Instruction

The included graphene liner is optimized for use with the factory-supplied MIG gun in pulse or non-pulse modes. For third-party liners/guns, verify compatibility to prevent feed issues or liner damage.

  1. Lay the MIG gun straight on a clean, flat surface.
  2. Remove all front-end consumables (nozzle, contact tip, gas diffuser).
  3. Unscrew the liner retaining nut at the torch base.
  4. Carefully pull the steel liner out of the gun cable assembly.
  5. Uncoil the new graphene liner and feed it gently into the gun cable, avoiding kinks.
  6. Attach the tip holder to the liner end and screw it into the torch neck. Tighten securely.
  7. Reinstall components in this order: Gas diffuser, special aluminum A+ contact tip, nozzle.
  8. Secure the liner retaining nut and O-ring at the torch base.
  9. Disengage the drive roller to free the wire feed mechanism.
  10. Remove the outlet guide tube and metal inlet guide tube.
  11. Feed the extended graphene liner into the Euro connector outlet guide tube hole.
  12. Route the liner over the drive roller and tighten the Euro connection.
  13. Trim excess liner with a sharp knife for a clean edge.
  14. Install a U-groove knurled drive roller (matched to your aluminum wire diameter).
  15. Replace the metal inlet guide tube with the graphene liner and reattach to the feeder.
  16. Load the aluminum spool and thread the wire through the liner.
  17. Power on the welder and select MIG/MAG mode from the Home Menu.
  18. Set parameters: Wire type (ALSI or ALMG), Gas (100% argon), Wire diameter (0.9mm), Pulse/non-pulse mode (pulse recommended for cleaner welds).

5.4. Flux-cored Welding Setup (FCAW)

The polarity adapter is located inside the machine, please wire it in FLUX GASLESS mode as shown above.

  1. Connect the MIG gun to the Euro Torch Connector on the welding machine.
  2. Secure the Wire Drive Polarity Lead to the Negative (-).
  3. Clamp the Work Clamp to the Positive (+), ensuring direct contact with clean, bare metal.
  4. Load the flux-cored wire spool into the cabinet.
  5. Thread the wire through the feeder and into the gun.
  6. Press the gun trigger or hold the Value Adjustment Knob to feed the wire through the gun until it extends slightly beyond the nozzle.
  7. Turn on the welder.
  8. Select Flux-Cored Welding Process from the Home Menu.
  9. Navigate to the Flux-Cored Parameter Settings page.
  10. Set Wire Diameter (0.8mm, 0.9mm, or 1.0mm) and Trigger Mode (2T, 4T, or Spot Welding).
  11. Confirm Standard MIG Gun Mode is active.

5.5. HF TIG Welding Setup (GTAW)

WARNING: TIG TORCH IS ALWAYS LIVE (ELECTRICALLY HOT). Use caution and ensure the TIG torch is not in contact with or close to a conductive or grounded material.

Note: Remove all connections from the Positive(+), Negative(-) Output Receptacle, and Torch Connector.

  1. Connect the TIG torch gas connector to the welder's Torch Connector.
  2. Plug the 5-pin torch control switch cable into the Trigger Connector Receptacle.
  3. Connect the work clamp to the welder's Positive (+) Output Receptacle.
  4. Attach the work clamp to the workpiece that needs welding.
  5. Set the tungsten electrode to stick out approximately 1/4 inch from the end face of the gas cup.
  6. Put the TIG torch away from all conductive materials.
  7. Install the gas hose into the Inlet for Argon Gas and connect to the gas pressure regulator (100% Argon only).
  8. Open the gas cylinder valve and adjust the gas pressure regulator to the correct flow rate (Recommend 20-35 CFH).
  9. Plug the power cable into a suitable power outlet.
  10. Turn on the power source and select TIG process.
  11. Press the Value Knob to set parameters and rotate the knob to adjust the values.
  12. Position the tungsten electrode 2-3 mm (0.08-0.12 in) above the workpiece, and trigger the torch control switch to initiate the welding arc using the HF technique.

REMEMBER TO CLOSE THE VALVE ON THE GAS CYLINDER IMMEDIATELY AFTER ALL WELDING IS COMPLETED.

Torch Assembling

  1. Ensure the Collet and Collet Body are sized to match your Tungsten Electrode diameter. Thread the Collet Body securely into the front end of the TIG Torch.
  2. Choose a Ceramic Nozzle size based on material thickness and shielding gas flow. Screw the nozzle onto the Collet Body until snug.
  3. Insert the Collet into the Collet Body. Slide the Tungsten Electrode through the collet, ensuring it is straight and centered.
  4. Thread the Back Cap onto the torch to lock the tungsten in place. Adjust the electrode so it extends 1/8" to 1/4" beyond the Ceramic Nozzle.

5.6. Plasma Cutting Setup

  1. Torch Installation: Connect the cutting torch to the Torch Connector and plug the 2-pin torch control switch cable into the Trigger Connector Receptacle.
  2. Work Clamp Setup: Attach the work clamp to the Positive (+) Output Receptacle. Ensure clamp contact is on clean, bare metal. Critical: Incorrect polarity will damage the machine.
  3. Air System Configuration: Install the air filter regulator between the air compressor and the machine's air inlet. Adjust the regulator to 60-90 PSI (4.0-6.2 bar).
  4. Workpiece Preparation: Securely clamp the workpiece to a stable surface. Position the cutting torch away from conductive materials.
  5. Power & Mode Selection: Plug the machine into a grounded power outlet. Turn on the machine and select CUT mode.
  6. System Check: Trigger the torch to verify airflow and pilot arc activation. Adjust airflow if uneven or sputtering.
  7. Set Cutting Parameters: Press the Value Knob to select parameters (e.g., current, pre-flow time). Rotate the knob to adjust values (refer to material thickness charts).
  8. Initiate Cutting: Hold the torch perpendicular to the workpiece, with the torch positioned above and in contact with the workpiece surface. Trigger the torch control switch to ignite the arc using the blowback technique. Maintain a steady travel speed for clean cuts.
Plasma cutting performance on metal

Figure 5.2: Powerful cutting performance, showing 10mm clean cut at 110V and 18mm at 220V.

5.7. Air Pressure Compressor Filter Regulator Installation

The ANDELI MIG-205DP Plasma Cutter offers dual air supply options for versatile cutting performance. An external air compressor delivers higher air pressure (PSI) for faster, cleaner cuts on thick materials, improving cut quality and sustaining prolonged cutting tasks.

Important Notes:

  • Regularly drain moisture from the pressure-reducing valve's water filter cup. Empty the cup immediately if the water level reaches 1/4 of its capacity.
  • Neglecting to drain moisture can degrade cut quality (increased dross, uneven edges) and damage internal components (e.g., valves, regulators).
  • Check the filter cup daily (or after prolonged use).
  • Store the compressor in a dry environment to minimize condensation.

6. Operation

6.1. Control Panel Introduction

The MIG-205DP features a user-friendly control panel with a 5-inch LED display and intuitive controls. Below is a guide to the main controls:

Control Panel Introduction with numbered buttons and knobs

Figure 6.1: Control Panel Layout.

  1. Gas Selection Button
  2. Preferences Button
  3. 2T/4T/Spot Welding Button
  4. Wire Ø (Wire Diameter Selection)
  5. Weld Mode
  6. Wire check function
  7. Encoder (for adjusting voltage/inductance/gas settings)
  8. Knob (for adjusting Fine Voltage/Welding Current & Voltage/Wire feed speed/Inductance)
  9. Europe Type torch connector
  10. Negative (-) Welding Output Terminal
  11. Polar conversion line
  12. Aviation socket for Cutting torch and TIG switch
  13. Positive (+) Welding Output Terminal
  14. CUT/ Negative (-) Welding Output Terminal
  15. Power Switch ON/OFF
  16. Power Input Cable with Plug
  17. Gas Connector
  18. Remote Welding Helmet Control Cable Connector
  19. Air Filter Mounting Bracket

6.2. MIG/MAG Welding Parameters

The MIG-205DP Synergic mode presets parameters by material thickness. Wire feed can be adjusted manually; current and voltage are automatic, with ±5V fine-tuning. Refer to the specifications section for recommended settings based on material and wire type.

Aluminum MIG welding showing weld beads on aluminum and carbon steel

Figure 6.2: Aluminum MIG Welding, suitable for aluminum alloy and carbon steel.

Aluminum Pulse MIG welding showing weld beads on aluminum and carbon steel

Figure 6.3: Aluminum Pulse MIG Welding for seamless welding of aluminum, steel, and stainless steel.

6.3. Flux-cored Welding Parameters

For optimal flux-cored welding results, select appropriate settings for specific welding applications. The table in the specifications section provides recommended voltage, wire diameter, and wire feed speed values for various materials. Adjusting these parameters based on the material and wire type ensures efficient performance and high-quality welds.

6.4. TIG Welding Parameters

The MIG-205DP supports HF TIG welding and Cold TIG welding. Refer to the TIG Electrodes Specification Reference Table in the specifications section for recommended current, tungsten color, diameter, filler metal, ceramic nozzle size, and gas flow rates.

HF TIG welding with cold mode and pulse function

Figure 6.4: HF TIG Welding, delivering versatile, long-duration welding with up to 205A output and HF non-contact ignition.

Cold TIG welding showing minimal distortion on thin stainless/carbon steel

Figure 6.5: Cold TIG Welding, minimizing distortion on thin stainless/carbon steel.

6.5. Plasma Cutting Parameters

The MIG-205DP features Non-Touch Pilot Arc for plasma cutting, which excels at cutting through challenging surfaces (rust, paint, or uneven textures) while minimizing slag production. Refer to the Cutting Setting Recommendation tables in the specifications section for optimal parameters based on material thickness.

6.6. MMA Welding Parameters

MMA (Manual Metal Arc Welding) is performed using a coated electrode. The machine supports stable arc ignition, smooth current output, and adjustable welding current. Refer to the Welding Current Guide and Electrode Polarity tables in the specifications section for recommended settings.

MMA welding with Hot Start, Arc Force, and Anti-Stick technology

Figure 6.6: MMA Welding, equipped with Hot Start, Arc Force, and Anti-Stick technology for reliable performance.

6.7. Weld Cleaning Function

The Weld Cleaning Mode is designed to clean and restore weld beads after welding, especially for stainless steel applications. It effectively removes surface oxides, discoloration, and heat marks without grinding or damaging the base material.

  1. Press the button to switch to Weld Cleaning Mode.
  2. Connect the cleaning torch control cable to the two-pin aviation socket on the welder.
  3. Connect the cleaning torch to the negative (-) terminal.
  4. Connect the ground clamp to the positive (+) terminal.
  5. Attach the brush tip to the cleaning torch and dip the brush into the cleaning solution.
  6. Place the brush so that it fully covers the weld bead.
  7. Rotate knob F to set amperage: 10-30A range.
  8. Press and hold the trigger on the cleaning torch, and move the torch steadily and evenly along the weld bead to clean the weld surface.

Note: After cleaning is completed, wipe the weld bead thoroughly with a damp cloth to remove any remaining cleaning solution.

Cleaning function showing before and after weld cleaning results

Figure 6.7: Weld Cleaning Function, showing before and after results.

7. Maintenance

Proper maintenance ensures the longevity and optimal performance of your ANDELI MIG-205DP welder.

7.1. General Maintenance

  • Keep the cabinet cover closed at all times unless adjusting wire or drive pressure.
  • Keep all consumables (contact tips, nozzles, and liner) clean and replace when necessary.
  • Replace INPUT POWER CABLE, ground cable, work clamp, or gun assembly when damaged or worn.
  • Avoid directing grinding particles towards the welder.
  • Periodically clean dust, dirt, grease, etc. from your welder using compressed air.
  • If using compressed air to clean the liner, DISCONNECT FROM POWER SOURCE.
  • Replace the wire feed drive roller when grooves are worn deep enough.
  • Check all cables periodically for good condition.
  • WARNING: ELECTRIC SHOCK CAN KILL! Always unplug the welder from its AC power source and wait several minutes for electrical energy to discharge before removing side panels.

7.2. Consumable Maintenance

It is crucial to maintain consumables to avoid premature replacement of the gun assembly.

  • Contact Tip: Always use a contact tip stamped with the same diameter as the wire. If wire burns back into the tip, remove and clean it. Replace if burned-back wire cannot be removed or if the hole is worn.
  • Nozzle: CAUTION: KEEP THE NOZZLE CLEAN! Clean spatter and slag buildup periodically. Failure to do so can damage the gun and lead to erratic welds, reduced penetration, and overheating. Test for a shorted nozzle by checking continuity between the contact tip and the outside of the nozzle with the welder unplugged.

8. Troubleshooting

This section provides guidance for identifying and resolving common issues. Always observe all safety guidelines.

8.1. General Alarms and Errors

Type Error Code Reason Solution
Over-Flow E-1 Load current too big or main power device under over-current protection. Restart welder. If warning remains, contact professional maintenance personnel.
Over-heat E-2 Over-working of main circuit. Do not power off; restart welding when overheat indicator stops lighting up.
Wire Feeder Fault E-3 Wire delivery machine abnormal. Check wire feeder circuit.
MIG adapter connection error protection E-8 CUT and TIG Status MIG adapter connected to fast socket. MIG adapter must not be connected to the fast socket.

8.2. Stick Welding Issues

Problem Possible Cause Course of Action
Poor starting Poor work clamp connection. Check and secure work connection.
Stick electrode blasts off when arc is struck Current may be set too high for electrode size. Adjust current.
Electrode "stick" in weld puddle Current may be set too low for electrode size. Adjust current.
Porosity (small cavities or holes from gas pockets in weld metal) Arc length too long. Reduce arc length.
Damp electrode. Use dry electrode.
Workpiece dirty. Remove all grease, oil, moisture, rust, paint, coatings, slag, and dirt from work surface before welding.
Excessive Spatter (scattering of molten metal particles that cool to solid form near weld bead) Amperage too high for electrode. Decrease amperage or select larger electrode.
Arc length too long or voltage too high. Reduce arc length or voltage.
Incomplete Fusion (failure of weld metal to fuse completely with base metal or a preceding weld bead) Insufficient heat input. Increase amperage. Select larger electrode and increase amperage.
Improper welding technique. Place stringer bead in proper location at joint during welding. Hold arc on groove side walls when weaving. Keep arc on leading edge of weld puddle.
Workpiece dirty. Remove all grease, oil, moisture, rust, paint, coatings, slag, and dirt from work surface before welding.
Lack Of Penetration (shallow fusion between weld metal and base metal) Improper joint preparation. Material too thick. Joint preparation and design must provide access to bottom of groove.
Improper weld technique. Keep arc on leading edge of weld puddle.
Insufficient heat input. Increase amperage. Select larger electrode and increase amperage. Reduce travel speed.
Burn Through (weld metal melting completely through base metal resulting in holes where no metal remains) Excessive heat input. Select lower amperage. Use smaller electrode. Increase or maintain steady travel speed.

8.3. TIG Welding Issues

Problem Possible Cause Course of Action
Poor starting No gas, incorrect gas flow. Check gas connection, cylinder valve, hoses, and torch. Set gas flow between 20-30 cfh.
Poor work clamp connection. Check & secure work clamp.
HF TIG doesn't initiate an arc Contaminated Tungsten. Grind to clean Tungsten.
Loose connection. Check all connectors and tighten.
Earth clamp not connected to work. Connect the work clamp directly to the work piece.
Incorrect Gas/Inadequate gas flow. Check gas cylinder contains pure Argon gas and is connected and the torch gas valve is open. Set the gas flow between 20-30cfh flow rate.
Tungsten burning away quickly Back cap not fitted correctly. Make sure the torch back cap is fitted so that the o-ring is inside the torch body.
Incorrect tungsten being used. Check and change the tungsten type if necessary.
Touching tungsten into the weld pool. Keep tungsten from contacting weld puddle. Raise the torch so that the tungsten is off of the work piece 3-6mm.
Contaminated tungsten Touching the filler wire to the tungsten. Keep the filler wire from touching the tungsten during welding, feed the filler wire into the leading edge of the weld pool in front of the tungsten.
Tungsten melting into the weld pool. Check that correct type of tungsten is being used. Too much current for the tungsten size so reduce the amps or change to a larger tungsten.

8.4. Cutting Issues

Problem Possible Cause Course of Action
The arc does not transfer to the workpiece Insufficient work clamp contact with the workpiece. Clean the area where the work clamp attaches to the workpiece. Inspect work clamp and lead for damage.
Improper cutting technique. Keep hand steady, touch tips on worksheet, start cut from edge.
Plasma torch may not be in contact with the workpiece. Physically drag the cutting nozzle on the workpiece as you cut.
Improper use of Plasma torch. Review operating instructions.
Poor cut quality Plasma torch parts are worn out. Examine consumables for wear and replace worn parts with new ANDELI consumable parts.
Moisture or oil in air supply. Install a moisture filter in the air supply line prior to machine.
Cutting speed too fast. Decrease your torch travel speed.
Plasma torch is too tilted. Ensure that Plasma torch head is perpendicular to the workpiece.
Workpiece is too thick. Choose thinner workpiece material within the operational limits of the plasma cutting machine.
Insufficient cut penetration Cutting current too low. Ensure plasma cutting machine has proper input power. If used, eliminate or reduce length of extension cord.
Plasma torch parts are worn out. Examine the consumables for wear and replace worn parts with new ANDELI consumable parts.
Non-genuine manufacturer's parts. Use only genuine ANDELI consumables for optimum performance.
Insufficient air flow or pressure. Check for obstructions blocking air flow and ensure 12 inches of clearance around vents.
Excessive dross Cutting speed too slow (bottom dross). Increase your torch travel speed.
Cutting speed too fast (top dross). Decrease your torch travel speed.
Cutting current too low. Ensure plasma cutting machine has proper input power. If used, eliminate or reduce length of extension cord.
Plasma torch parts are worn out. Examine the consumables for wear and replace worn parts with new ANDELI consumable parts.
Non-genuine manufacturer's parts. Use only genuine ANDELI consumables for optimum performance.
Air pressure too low. Inspect air compressor, airlines, and filters for proper operation. Inspect consumables for obstructions and proper installation.
Exceeding plasma cutting machine capability (material too thick). Choose thinner workpiece material within the operational limits of the plasma cutting machine.
Excessive wear of the cutting nozzle or electrode Moisture or oil in air supply. Install a moisture filter in the air supply line prior to machine.
Improperly assembled or loose Plasma torch consumables. Check Plasma torch consumables for proper installation.
Damaged Plasma torch consumable. Check plasma torch consumables for damage and replace if damaged.
Non-genuine manufacturer's parts. Use only genuine ANDELI consumables for optimum performance.
Tilted cut edge angle (not perpendicular) Plasma torch position not correct. Ensure that plasma torch head is perpendicular to the workpiece.
Workpiece thickness is near the capacity of the machine. Cut thinner material. 12mm thick material cuts will not have a clean cut edge.
Asymmetric wear of cutting nozzle hole or wrong assemblage of the plasma torch parts. Check plasma torch consumables for wear and proper installation. Examine the consumables for wear and replace worn parts with new ANDELI consumable parts.

9. Wiring Diagram

For detailed internal wiring, please refer to the diagram below. This diagram is for qualified technicians only.

Internal wiring diagram for the ANDELI MIG-205DP welder

Figure 9.1: Internal Wiring Diagram.

10. User Tips

  • For thin materials, especially stainless steel, utilize the Cold Welding (TIG mode) to minimize distortion and discoloration.
  • When performing plasma cutting on painted, rusty, or uneven surfaces, the HF pilot arc ensures stable cutting performance without needing to touch the workpiece.
  • Take advantage of the Synergic MIG mode for automatic parameter matching, which simplifies setup for common welding tasks. However, remember you can fine-tune parameters manually for specific needs.
  • Regularly check and clean the air filter regulator, especially when using the plasma cutting function, to ensure consistent airflow and prevent damage to internal components.
  • The machine's ability to automatically memorize welding parameters can save time between jobs; ensure you understand how to restore previous settings if needed.

11. Product Demonstration Video

Watch this video for a visual guide on the features and operation of the ANDELI MIG-205DP Multi-Process Welder.

Video 11.1: ANDELI MIG-205DP Multi-Process Welder in action, demonstrating various welding and cutting modes.

ANDELI Official Store

For further assistance, please contact support@andeligroup.com

Documents and downloads

Ask a question about this manual

Ask about setup, troubleshooting, compatibility, parts, safety, or missing instructions. Manuals+ will review the question and use this page’s manual context to help answer it.